Skip to content

Setting up Process Profile

Note

Speed changes in Other layers speed and First layer speed should be based on the filament you are using recommendations. Below is my Sunlu PLA settings.

  1. Click speed tab.

    OrcaSlicerProcessSpeedTab.png

  2. Scroll down to First layer speed section.

  3. In First layer speed section.
  4. Change you should change these:

    • First layer: 25
    • First layer infill: 45
    • Number of slow layers: 3 (can be 2, but I found 3 working the best, for me)

    OrcaSlicerProcessFirstLayer.png

  5. Scroll down to Other layers speed

  6. In Other layers speed change these:

    • Outer wall: 45
    • Inner wall: 75
    • Spare infill: 75
    • Internal solid infill: 75
    • Top surface: 50
    • Gap infill: 30

    OrcaSlicerProcessOtherLayersSpeedSunlu.png

  7. Scroll down to Travel speed

  8. Set:
    • Travel: 2500
  9. Scroll down to Acceleration
  10. Set:

    • Normal printing: 0

    OrcaSlicerProcessTravelSpeedAndAcceleration.png

  11. Scroll down to Jerk(XY)

  12. Set:
    • default: 0
  13. Click save icon.
  14. Name the profile. My recommendation is to use this naming schema: Brand+filament type, for example Sunlu PLA
  15. Click User preset
  16. Click ok.

    OrcaSlicerProcessSave.png